UJI KELAYAKAN KUALITAS PASIR SUNGAI MAUBESI DENGAN PASIR LUMAJANG TERHADAP KUAT TEKAN BETON DAN KUAT TARIK BETON ( MUTU FC’ 25 MPa) Handika Setya Wijaya; Blasius Tahik
Jurnal Qua Teknika Vol 10 No 2 (2020): September 2020
Publisher : Universitas Islam Balitar Blitar

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.35457/quateknika.v10i2.1199

Abstract

Aggregate needs in Maubesi, North Central Timor Regency, , as a concrete mixture for the work of construction of natural stone, which has quite a large potential. Research is aimed at; 1) know the characteristics of the statical river in the Maubesi, North Central Timor Regency, and aggregate dulcet from Lumajang; 2) find to uncover of the pressure concrete and the pull that has been generated from the river of North East Timor Regency and the aggregate dulcet of Lumajang; 3) find out the modulus of elasticity of the rivers of the from river in the Middle East North Coast and the Lamajang . This research is a collaborative research on the sample base and analysis of aggregate characteristics and testing of basic conditions and tests interested in and modulus of elasticity. Aggregates Strong pressure from the basement to the beginning until the end is obtained from the 2.747 walk in zone 1 ( fine send ) aggregate North Center of Central Timor, with the strength of Central Timor in the amount of 13,472 MPa ( congrete age ) silkiness of the (concrete age 7 days) , 20,727 MPa (concrete age 28 days), The compressive strength of concrete from the initial age of concrete to the end was obtained from the Maubesi aggregate of North Central Timor with compressive strength of 13,472 MPa (concrete age of 7 days), 20,727 MPa (concrete age of 28 days), and strength Tensile pull of 1,529 MPa (7 days concrete age), 2,352 MPa (28 day concrete age). While the compressive strength of concrete is obtained from the aggregate. Lumajang with compressive strength totaling 18,072 MPa (7 days concrete age), 27,802 MPa (28 days concrete age), and Tensile strength of aggregate rolled concrete. , 3,297 MPa (concrete age 28 days). Modulus of elasticity of the Maubesi North Central Timor aggregate 25677.1 N / mm² while for Lumajang aggregate 25385.9141 N / mm²
PENGARUH PENAMBAHAN LIMBAH BAN BEKAS TERHADAP KEKUATAN BETON Handika Setya Wijaya; Evangelino Da Cruz Evangelino
Jurnal Qua Teknika Vol 11 No 1 (2021): Maret 2021
Publisher : Universitas Islam Balitar Blitar

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.35457/quateknika.v11i1.1405

Abstract

In the world of construction, concrete still plays an important role as the main material used. This is because concrete has several advantages such as ease of work, the use of solid waste as material substitution in the industry is not new. However, the use of solid waste as a substitute for aggregates in concrete has been increasing in recent years, as a promising solution to reduce inorganic solid waste. From the tests carried out in the university tribhuwana to laboratories, it shows that for compressive strength and tensile strength, it decreases. The concrete compressive strength test results with added material in the form of tire chips and in the testing of compressive strength for 5% used tire waste burned 13.22 MPa, as well as 10%, the value burned 9.74 MPa, and for compressive strength test 15% of the value decreases for compressive strength with a mixture of burnt tire chips 4.77Mpa. The graph of the concrete tensile strength test with added material is in the form of tire chips and in testing the tensile strength for used tire waste 5% with for concrete that is not burned 1.844Mpa value. Likewise with 10% for unburned concrete the value of 2,020Mpa with a mixture of used tire waste as added material. And for the tensile strength test 15% the value decreases for non-burned concrete with a quality of 1.544Mpa.