Thermoluminescence response of TLD CaSO4: Dy with a variation of the addition of SiO2 and PTFE materials has been observed. TLD CaSO4:Dy derived through co-precipitation method and then added by SiO2 and PTFE. Thermoluminescence intensity for CaSO4:Dy added by SiO2 obtained 9.41, 5.32; and 13.93 nC for the temperature at 400 °C, 600 °C and 700 °C. As for CaSO4:Dy with the addition of PTFE obtained 33.10; 336.89; and 1191.11 nC for the temperature at 400 oC temperature, 600 °C and 700 °C. Thermoluminscence intensity for CaSO4:Dy without the addition of SiO2 and PTFE at a temperature of 700 °C is 75.15 nC. There’s a significant increasing in the thermoluminescence intensity on CaSO4:Dy added by PTFE.