Pengaruh Kondisi Wire Top Flat pada Mesin Carding Meikin terhadap Jumlah Neps dan Ketidakrataan Sliver

Hamdan S Bintang (Unknown)
Fajar Pitarsi Dharma (Unknown)
Dwi Wahyu Hidayat (Unknown)



Article Info

Publish Date
01 Jul 2021

Abstract

Berdasarkan pengamatan teknis melalui diagram fishbone terdapat beberapa faktor yang menyebabkan tumpulnya wire top flat. Solusi yang dilakukan untuk menyelesaikan kasus ini adalah penyelesaian teknis dengan cara melakukan penggrindaan terhadap wire top flat sehingga kondisi wire kembali tajam dan kualitas sliver yang dihasilkan meningkat. Penggrindaan sendiri bertujuan untuk mempertajam kembali wire yang telah tumpul. Akan tetapi, apabila wire mengalami over grinding atau penggrindaan berlebih akan menyebabkan wire menjadi melengkung. Wire yang melengkung dapat menyebabkan serat-serat tersangkut pada wire yang melengkung tersebut. Based on the technical assessment through the fishbone diagram, there are several factors that cause the bluntness of the wire top flat. The solution takes to solve this case is a technical solution by grinding the top Flat wire so that the wire condition becomes sharp again and the resulting sliver quality increases. Grinding itself aims to sharpen the wire that has been blunt. However, if the wire is over-grinding or over-grinding it will cause the wire to warp. Curved wire can cause the fibers to get caught in the curved wire.

Copyrights © 2021






Journal Info

Abbrev

jurnal

Publisher

Subject

Decision Sciences, Operations Research & Management Engineering Industrial & Manufacturing Engineering Materials Science & Nanotechnology Mechanical Engineering

Description

Jurnal Teksil (JUTE) ISSN 2797-9229(online) is a peer-reviewed Open Access Journal (OJS) that publishes original research articles as well as review articles in several engineering fields. The subject areas covered by this journal covers broad themes in the fields of textile, apparel and garment, ...