cover
Contact Name
Dr. Ratih Damayanti
Contact Email
ratih_turmuzi@yahoo.com
Phone
+622187914511
Journal Mail Official
ejournal_wrj@gmail.com
Editorial Address
Research Center for Biomaterials,Indonesian Institute of Sciences Jl. Raya Bogor Km 46, Cibinong, Bogor 16911, Indonesia
Location
Unknown,
Unknown
INDONESIA
Wood Research Journal : Journal of Indonesian Wood Research Society
ISSN : 20873840     EISSN : 27749320     DOI : 10.51850/wrj
Core Subject : Agriculture,
Wood Research Journal is the official journal of the Indonesian Wood Research Society. This journal is an international medium in exchanging, sharing and discussing the science and technology of wood. The journal publishes original manuscripts of basic and applied research of wood science and technology related to Anatomy, Properties, Quality Enhancement, Machining, Engineering and Constructions, Panel and Composites, Entomology and Preservation, Chemistry, Non Wood Forest Products, Pulp and Papers, Biomass Energy, and Biotechnology. Besides that, this journal also publishes review manuscripts which topics are decided by the Editors.
Articles 5 Documents
Search results for , issue "Vol 11, No 2 (2020): Wood Research Journal" : 5 Documents clear
Improving Fire Resistance of Mahogany (Swietenia macrophylla) Wood Impregnated with Mixture of Borax and Boric Acid Tomy Listyanto; Aditya Aji Pratama; Keisuke Ando; Nobuaki Hattori
Wood Research Journal Vol 11, No 2 (2020): Wood Research Journal
Publisher : Masyarakat Peneliti Kayu Indonesia

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.51850/wrj.2020.11.2.48-52

Abstract

The study was aimed to investigate the effects of mixture of borax and boric acid concentration and different level of pressure on absorption, retention quantity, and fire resistance properties of mahogany (Swietenia macrophylla). A total of 50 samples of 9 x 19 x 1016 mm (ASTM E 69-02) were taken from mahoganylumber and then air-dried. A total of 45 samples were impregnated with aqueous solutions of borax and boric acid in three different concentrations (5, 7, and 9 %) and at three different pressure levels (5, 7.5, and 10 atm) for 2 hours pressure time, while5 samples were liftedas control. Dried impregnated samples and untreated samples were feeding in flame with lid combustion method refers to ASTM E 69-02. Interestingly, the results showed that borax and boric acid effectively improved the fire resistanceproperties(mass losses, ignition temperature, maximum temperature, and smoke and smolder production)of mahogany wood.Mixtures of borax and boric acid at a concentration level of 9% and pressure of 10 atm arerecommended to obtain the best results compare to the other interactions on combustion properties.
Reduction in Toxicity of Tectoquinone against Reticulitermes speratus Kolbe termites Ganis Lukmandaru
Wood Research Journal Vol 11, No 2 (2020): Wood Research Journal
Publisher : Masyarakat Peneliti Kayu Indonesia

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.51850/wrj.2020.11.2.58-64

Abstract

The cause of low toxicity against Reticulitermes speratusKolbe termite species of teakwood under natural condition was investigated. Anti-termite test was conducted to evaluate the effectivity of four major components (tectoquinone, deoxylapachol, tecomaquinone, and squalene) of ethanol-benzene extracts in the teak heartwood. Tectoquinone exhibited both strong toxicity and antifeedancy as well as it was far superior to other components. The strength reduction of tectoquinone bioactivity is assumed due to interaction with other major components. As squalene was found in considerable amounts or 1.8 to 13.1 times as high as the tectoquinone concentration in woods, termite feeding was set to the mixtures of tectoquinone and squalene in various ratios (1:1, 1:5, 1:10, and 1:20). It was revealed that squalene addition could decrease the termite mortality 15% to 44% from its initial value (tectoquinone only). On the other hand, the mixtures reduced mass loss due to termite attacks only to a small degree.
Antifungal Activity of Triterpenoids and Steroids Isolated from Pinus merkusii Bark Against Phanerochaete chrysosporium Masendra Masendra; Brandon Arsito Verick Purba; Ganis Lukmandaru
Wood Research Journal Vol 11, No 2 (2020): Wood Research Journal
Publisher : Masyarakat Peneliti Kayu Indonesia

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.51850/wrj.2020.11.2.65-71

Abstract

The outer part of a tree, known as the bark, protects the internal tissues from external conditions and attacks from microorganisms. Its antifungal activities are due to the presence of chemicals in this bark. This study aimed at evaluating the toxicity of triterpenoids and steroids from the bark of Pinus merkusii against Phanerochaete chrysosporium (white-rot). The triterpenoids and steroids were isolated from n-hexane extract of the bark through column chromatography. Then, the antifungal activity was evaluated by measuring the growth rate of the fungus on potato dextrose agar (PDA) medium in a Petri dish. The isolation resulted in three triterpenoids (3β- methoxyserratt-14-en-21-one, serrate-14-en-3β,21β –diol, 3α,21β- dimethoxy-D14-serratene) and two steroids (β-sitosterol, Stigmast-4-en-3-one). There was more of antifungal activity with β-sitosterol and serrate-14-en-3β,21β –diol, due to presence of hydroxyl bond and their hydrophobicity.
Strength and Stiffness Behavior of Earthquake Resistant Pedestrian LVL Timber Bridge Bernardinus Herbudiman; Delima Delima; Yosafat Aji Pranata
Wood Research Journal Vol 11, No 2 (2020): Wood Research Journal
Publisher : Masyarakat Peneliti Kayu Indonesia

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.51850/wrj.2020.11.2.53-57

Abstract

A bridge is a structure which is used to connect two areas separate by obstacles. The environmental damage caused a number of reductions in the production of timber, and by that, the LVL timber which is a high quality processed or engineered timber is chosen. This research determined the design of the timber bridge structure for pedestrian with simple beam type and earthquake resistant. The load in this bridge is referring to the SNI 1725:2016 and SNI 2833:2008, the design of the girder and the connection is referring to SNI 7973:2013, and the deflection is referring to the LFRD for Highway Bridge Superstructures. The timber bridge is designed to have a span of 10 metres long and 3 metres wide. The modeling and designing of the wooden bridge are using an application called SAP2000 based on finite element analysis. Result obtained from this research indicated that the longitudinal dimension of the girder is 360 mm x 630 mm and the cross sectional dimension is 180 mm x 270 mm. The number of bolts and lock screws needed on the connection among the longitudinal girders are 40 pieces, between the longitudinal girders and the cross sectional girders is three pieces, and between the railing and the slab are two pieces. Based on the stiffness review, the results showed that the bridge deflection that occurred was lower than the permit deflection
Wood Permeability Assessment of Young Teak (Tectona grandis L.f.) Ratih Damayanti; Krisdianto Krisdianto; Jugo Ilic; Gustan Pari; Peter Vinden; Barbara Ozarska
Wood Research Journal Vol 11, No 2 (2020): Wood Research Journal
Publisher : Masyarakat Peneliti Kayu Indonesia

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.51850/wrj.2020.11.2.41-47

Abstract

Wood properties of young teak (Tectona grandis L.f.) is inferior, and then preservative treatment is one possible solution to enhance its service life. The uptake and movement of preservatives through wood cell structure is directly connected to the wood permeability. There are two simple methods to identify wood permeability: water soaking and bubble test methods. This paper assesses the young teak permeability by water soaking and bubble test methods. The assessment was conducted into five cm thick young-teak discs by soaking in the red-dye water and blowing air into the discs which had been coated with soap. Results show that the heartwood is less permeable than sapwood. Red-dye penetrates almost 100% of the sapwood area, and the red-dye did not penetrate in the heartwood. Red-dye only penetrates in the cracked heartwood through the void volume in the cracking heartwood. There is a transition zone between sapwood and heartwood, and it is refractory. Bubble test with air pressure from compressor could open the air-pathway in the heartwood and sapwood of young-teak discs taken from Bogor. The bubble test result of young-teak discs from Madiun showed air-pathway only in the sapwood, but heartwood. The air pressure is not capable of moving the vapour through the wood cell. It indicates that the heartwood of young-teak from Madiun is less permeable and less possibility for pressure treatment.