Degrees of chitosan deacetylation from white shrimp shell waste as dental biomaterials Sularsih Sularsih; Anita Yuliati; Coen Pramono D
Dental Journal (Majalah Kedokteran Gigi) Vol. 45 No. 1 (2012): March 2012
Publisher : Faculty of Dental Medicine, Universitas Airlangga https://fkg.unair.ac.id/en

Show Abstract | Download Original | Original Source | Check in Google Scholar | Full PDF (318.046 KB) | DOI: 10.20473/j.djmkg.v45.i1.p17-21

Abstract

Background: Chitosan is biomaterial improved for various dentistry applications because it is biocompatible, degradable, nontoxic, and not carcinogenic. The main parameter affecting the characteristics of chitosan is deacetylation degree. Purpose: This study is aimed to determine the degree of deacetylated of chitosan derived from white shrimp shell waste used as dental biomaterial. Methods: White shrimp shells were crushed into powder. Next, deproteination process was conducted with 3.5% NaOH solution, demineralized with 1N HCl solution, and then depigmented with 90% acetone solution into chitin powder. Deacetylation process was then conducted by soaking the chitin powder in 50% NaOH solution for 6 h at 65° C to produce white powder of chitosan. Afterwards, deacetylation degree test was conducted by using Fourier Transform Infrared Spectrophotometer (FTIR) to calculate the ratio of the absorption bands between the absorbance peak of amide group about 1655 cm–1 and the absorbance peak of hydroxyl group about 3450 cm–1. Results: The result of the deacetylation degree test on the chitosan powder derived from white shrimp shell waste was high, about 85.165%, and had the eligible form, solubility, and pH. Conclusion: It can be concluded that the deacetylation degree of chitosan from white shrimp shells could reach 85.165%.Latar belakang: Kitosan merupakan biomaterial yang dikembangkan untuk berbagai aplikasi kedokteran gigi karena biokompatibel, dapat didegradasi, tidak toksik dan tidak karsinogenik. Parameter utama yang mempengaruhi karakteristik kitosan adalah derajat deasetilasi. Tujuan: Tujuan dari penelitian ini adalah mengetahui derajat deasetilasi kitosan dari limbah kulit udang putih sebagai biomaterial kedokteran gigi. Metode: Kulit udang putih dihaluskan menjadi serbuk. Setelah itu dilakukan proses deproteinasi dengan larutan NaOH 3,5%, demineralisasi dengan larutan HCl 1N, depigmentasi dengan larutan aseton 90% sehingga menjadi serbuk kitin. Proses deasetilasi dilakukan dengan merendam serbuk kitin dalam larutan NaOH 50% selama 6 jam pada suhu 65° C sehingga dihasilkan serbuk putih kitosan. Uji derajat deasetilisasi menggunakan metode spektrofotometer Fourier Transform Inframerah (FTIR) dengan menghitung nilai perbandingan pita serapan antara puncak absorbansi gugus amida sekitar 1655 cm–1, dan puncak absorbansi gugus hidroksil sekitar 3450 cm–1. Hasil: Hasil uji derajat deasetilasi serbuk kitosan dari limbah kulit udang putih adalah tinggi yaitu sebesar 85.165% dan memiliki bentuk, kelarutan dan pH yang memenuhi syarat. Kesimpulan: Dapat disimpulkan derajat deasitilasi kitosan dari kulit udang putih adalah 85,165%.
Expression of bone morphogenetic protein-2 after using chitosan gel with different molecular weight on wound healing process of dental extraction Sularsih Sularsih; Endah Wahjuningsih
Dental Journal (Majalah Kedokteran Gigi) Vol. 48 No. 2 (2015): June 2015
Publisher : Faculty of Dental Medicine, Universitas Airlangga https://fkg.unair.ac.id/en

Show Abstract | Download Original | Original Source | Check in Google Scholar | Full PDF (1399.431 KB) | DOI: 10.20473/j.djmkg.v48.i2.p53-58

Abstract

Background: Bone morphogenetic protein-2 (BMP-2) is bone stimulator which capable of inducing differentiation of mesenchymal cells into osteoblast, stimulating bone formation in wound healing process of dental extraction. Chitosan is polymer composed N-acetylD-glucosamine unit that has been used in various applications in wound healing process and bone tissue engineering. Purpose: The objective of this research was to analyzed expressions of BMP-2 for 7,14 and 21 days after using chitosan gel with different molecular weight on wound healing process of dental extraction. Method: The research was an experimental laboratory study. Rattus nornegicus strain wistar male, aged 8-16 weeks, divided into 3 treatment groups namely group 1 and II which given chitosan gel 1 % with high and low molecular weight and group III as control which were not given chitosan gel. Chitosan gel were applied into the socket of dental extraction. Rat was decaputated 7,14 and 21 days after chitosan gel application and the jaw in the treated regions and control group were cut for immunohistochemical examination to observe BMP-2. Data were analyzed using ANOVA test. Result: The result of this research showed significant differences on BMP-2 for 7,14 and 21 days observation (p<0,05). The increasing of BMP-2 were found in the group which given chitosan gel with high molecular weight. Conclusion: It may be concluded that chitosan gel with high molecular weight can enhance the expresion of BMP-2 on wound healing process ofdental extraction.
The pore size of chitosan-Aloe vera scaffold and its effect on VEGF expressions and woven alveolar bone healing of tooth extraction of Cavia cobaya S. Sularsih
Dental Journal (Majalah Kedokteran Gigi) Vol. 53 No. 3 (2020): September 2020
Publisher : Faculty of Dental Medicine, Universitas Airlangga https://fkg.unair.ac.id/en

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.20473/j.djmkg.v53.i3.p115-121

Abstract

Background: Pore size of scaffolds affects cellular activity, stimulates angiogenetic factors of vascular endothelial growth factor (VEGF), synthesises new blood vessels to regulate migration and proliferation, and accelerates alveolar bone healing of tooth extraction. Purpose: This study aims to analyse the pore size of chitosan-Aloe vera scaffold and its effects on VEGF expression and woven alveolar bone healing of tooth extraction of Cavia cobaya. Methods: 36 male Cavia cobaya, aged 3-3.5 months were divided into six groups: negative control groups (without scaffold), positive control groups (chitosan scaffold), and treatment groups (chitosan-Aloe vera scaffold) on 7- and 14-day observations. Histopathological examination was performed to account the woven alveolar bone areas, and immunohistochemical examination was conducted to examine VEGF expressions on endothelial cells. Data was analysed using a one-way analysis of variance (ANOVA) and least significant difference (LSD) test (p<0.05). Scaffold pore size examination was performed with scanning electron microscope (SEM) with 250x and 500x magnification. Results: Chitosan-Aloe vera scaffold was found to have open pore interconnectivity, the largest pore size was 138.9 μm, while the smallest was 110.5 μm and average pore size was 134.85 μm. The highest expression of VEGF was observed in the treatment group on days 7 (11.5 ±1.39)  and 14 (15.28±1.78), while the largest woven alveolar bone was observed in the treatment group on days 7(17.83±1.47) and 14 (37.67±3.65). Statistically, there was a significant difference between control groups and the treatment groups (p=0.000; p<0.05). Conclusion: Chitosan-Aloe vera scaffold has pore characteristics increasing VEGF expressions and woven alveolar bone areas.